Production standards:
High coating adhesion, no spalling of coating, no micro chipping of cutting edge, Five inspections to ensure production standards.
Five inspections:
→1. Mixed material inspection. → 2. Blank inspection after pressing. →3. Blank inspection after sintering.
→4. Blank inspection before coating. →5. Full inspection of finished product after coating
Grade recommendation | Grade Introduction | Always stock available | Vc | Fn | Ap |
YC331 | 1. High wear resistance substrate 2. Thick AL2O3 coating 3. Improved impact toughness 4.substantially improved wear resistance 5.the first choice for steel general machining. | CNMG120404-WM | 200(160-320) | 0.2(0.05-0.4) | 1.0(0.1-2.0) |
CNMG120408-WM | 200(160-320) | 0.2(0.05-0.4) | 3.0(1.0-5.0) | ||
CNMG120412-WM | 200(160-320) | 0.2(0.05-0.4) | 4.0(1.5-6.0) | ||
YC333 | 1. High wear resistance substrate 2. Thick AL2O3 coating 3. Improved impact toughness 4. substantially improved wear resistance 5. the first choice for steel general machining. | CNMG120408-WM | 200(160-320) | 0.2(0.05-0.4) | 1.0(0.1-2.0) |
CNMG120408-WM | 200(160-320) | 0.2(0.05-0.4) | 3.0(1.0-5.0) | ||
CNMG120412-WM | 200(160-320) | 0.2(0.05-0.4) | 4.0(1.5-6.0) | ||
Matching tool holder | |||||
MCBNR/L | MCLNR/L | S-type-MCLNR/L |